What is the welding procedure for ASTM A588 Gr.A weathering steel

What is the welding procedure for ASTM A588 Gr.A weathering steel

Different from ordinary steel plates, ASTM A588 Gr.A weathering steel has good corrosion resistance. Under severe weather such as acid rain, many buildings began to show different degrees of corrosion, which not only affected the buildings, but also affected the people in the buildings. At the same time it also brings some security risks.

1. Process the grooves in the welds of ASTM A588 Gr.A weathering steel and stainless steel plates respectively;

2. After polishing and removing the dirt around the groove, pair the groove of ASTM A588 Gr.A weathering steel with the groove of the stainless steel plate to form a welding area;

3. Non-pulsating solder is used in the weld zone formed between ASTM A588 Gr.A weathering steel and the stainless steel plate to form a primer layer at the lower part of the weld zone;

4. Non-pulsating solder is used to cover the upper surface of the soldering layer in the soldering zone to form a covering layer in the ASTM A588 Gr.A weathering steel soldering area. By welding weather-resistant plates and stainless steel plates under low current and voltage, reducing the heat of ASTM A588 Gr.A weathering steel and stainless steel during the welding process, effectively reducing the melting rate of the two plates, and manufacturing ASTM A588 Gr.A weathering steel and stainless steel. It can be more completely fused to improve the weldability of welding.

Leave a Comment

If you have any need about our steel products, Please send email to [email protected] or leave a message to use this function. we will reply you ASAP!

Technology

Contact Us

  • Address: Xichen Science & Technology Building High-tech Development Zone, Zhengzhou, China
  • Tel: 0086-371-86151827
  • Fax: 0086-371-86011881
  • Email: [email protected]
Looking for Corten A steel, weathering steel plates? BBN Group is a good choice.
div style="display:none;">